Battery knowledge · Safety and abuse

Onset temperature

The temperature at which a cell begins to generate heat by itself, as the SEI starts to decompose, typically 80–120 °C. Measured in an accelerating rate calorimeter, it marks the start of the path to thermal runaway, not the runaway itself.

Also called
self-heating onset
Unit
°C

Example

Safety and abuse: an example situation

A low normal-load temperature does not demonstrate thermal-runaway containment.

Read Onset temperature alongside Accelerating rate calorimetry in this context. A test in which a cell sits in an adiabatic chamber that follows its temperature, so any self-heating is not lost to the surroundings. It measures the onset temperature, the self-heating rate and the temperature at which runaway becomes unstoppable.

Use in Lemonergy

Connect mechanisms with appropriate test evidence.

This is a reference concept. No executable Lemonergy block has been verified for this term.

References & further reading

Further reading on this topic

These sources provide broader context; they are not presented as citations for every statement in this entry.

  1. Thermal runaway mechanism of lithium ion battery for electric vehicles: A review

    Xuning Feng et al. · Energy Storage Materials · 2018

    Topic background · Electrical, mechanical and thermal abuse; thermal-runaway mechanisms and propagation.